An Experiment of How the Length and the Diameter of the sprue Effects the Size of the porosity, that is Created During the Moduling Process
Hwang Seung-Sig

Abstract
This experiment was done to find out how the length and the diameter of the sprue effects the porosity created during the moduling process, which is caused by the metal¡¯s shrinking and stretching action. the experiment was done in two groups(A and B), using experimental gold, and made 10 copings for both groups. 1. In group A, The length of the sprues were given the same, but the diameter of the sprue were 6, 8, 10, 12, 18 gauge. As a result, the porosity came out big with 12 and 18 gauge and for 10, 8, 6 gauge, the porosity was hardly seen or none was noticeable. 2. In group B, the diameter was given the sam for the sprues, but the length of the sprues were 5, 10, 15, 20, 25mm. As a result, the porosity came out big with 25, 20, 15mm the porosity was hardly seen or none was noticeable. 3. The diameter needs to be big and the length, short. 4. The appropriate sized sprue must be chosen for each individual tooth, according to it¡¯s shape and size.
KEYWORD
FullTexts / Linksout information
Listed journal information
ÇмúÁøÈïÀç´Ü(KCI)