Àá½Ã¸¸ ±â´Ù·Á ÁÖ¼¼¿ä. ·ÎµùÁßÀÔ´Ï´Ù.
KMID : 0362220130400020137
Journal of The Korean Research Society for Dental Materials
2013 Volume.40 No. 2 p.137 ~ p.142
Microshear Bond strength of Self-adhesive Resin Cement to Universal primer-treated Zirconia
Lee Lin-Jie

Lee Du-Hyeong
Kwon Tae-Yub
Jin Myoung-Uk
Lee Kyu-Bok
Abstract
The objective of the study was to evaluate conventional and self-adhesive resin cements bonding to zirconia ceramic that were sandblasted and primed with universal primer. 8 sintered zirconia ceramic disks (Ceramill Zolid; Amann Girrbach, Austria) were air-abraded with 110 §­ Al©üO©ý at 2.5 bar pressure for 15s at a distance of 10 §® and ultrasonic cleaned in 95% alcohol for 3min. All the specimens were applied by universal primer 60s and dried. The primed specimens were divided into 4 groups (n=10) according to the resin cement used: RelyX Unicem, Multilink Speed, MaxCem Elite) Panavia F2.0. The resin cement cylinders were stored in distilled water at 37¡É for 24h. Microshear bond strength (MSBS) test was measured with a universal testing machine. The means and standard deviations of microshear bond strength for RelyX Unicem, Multilink Speed, MaxCem Elite, Panavia F2.0 were 18.57 (4.80), 8.21 (4.95), 4.59 (3.14), 4.61 (2.80) MFa, respectively. Statistical analysis revealed that the MSBS of RelyX Unicem, Multilink Speed were significantly higher than MaxCem Elite, Panavia F2.0 (p£¼0.05). When self-adhesive resin cement bond to zirconia, universal primer plays a role of improving the bond strength to zirconia. It is recommended to use RelyX Unicem, Multilink Speed bond to zirconia which is primed with universal primer.
KEYWORD
Self-adhesive resin cement, zirconia, universal primer, microshear
FullTexts / Linksout information
 
Listed journal information
ÇмúÁøÈïÀç´Ü(KCI)