Effect of Hydride Reorientation on Delayed Hydride Cracking In Zr-2.5Nb Tubes
Yun, Yeo Bum
Kim, Young Suk/Im, Kyung Soo/Cheong Yong Moo/Kim, Sung Soo
Abstract
KEYWORD
Zr-2.5Nb, reorientation, hydrides, delayed hydride cracking (DHC), supersaturation, hydrogen