On-Site Corrosion Behavior of Water-Treated Boiler Tube Steel
Seo Jung-hwa

Choi Mi-hwa
Yinsheng He
Yang Seok-Ran
Lee Je-Hyun
Keesam Shin
Abstract
The boiler tubes of X20CrMoV12.1 used in fossil-fired power plants were obtained and analyzed for the effect of water treatment on the steam corrosion-induced oxide scale in an effort to better understand the oxide formation mechanism, as well as pertinent method of maintenance and lifetime extension. The specimens were analyzed using various microscopy and microanalysis techniques, with focuses on the effect of water treatment on the characters of scale. X-ray diffraction analysis showed that the scales of specimens were composed of hematite (Fe2O3), magnetite (Fe3O4), and chromite (FeCr2O4). Electron backscatter diffraction analysis showed that the oxides were present in the following order on the matrix: outer Fe2O3, intermediate Fe3O4, and inner FeCr2O4. After all volatile treatment or oxygenated treatment, a dense protective Fe2O3 layer was formed on the Fe3O4 layer of the specimen, retarding further progression of corrosion.
KEYWORD
All volatile treatment, Oxygenated treatment, Boiler tube, Corrosion behavior, Electron microscopy
FullTexts / Linksout information
 
Listed journal information
ÇмúÁøÈïÀç´Ü(KCI)