KMID : 0613320090150020093
Journal of the Korean Bone and Joint Tumor Soceity
2009 Volume.15 No. 2 p.93 ~ p.103
Reconstruction of Bone Defects Caused by Tumor Resection Using Recycled Autograft Augmented with VFG
Chung Yang-Guk

Kang Yong-Koo
Park Won-Jong
Rhee Seung-Koo
Lee An-Hi
Park Jeong-Mi
Park Bo-Youn
Abstract
Purpose: We evaluated the outcomes of surgical reconstructions using recycled autograft augmented with VFG for bone defects caused by tumor resections.

Materials and Methods : Ten patients with a malignant or locally aggressive bone tumor who were managed with recycled autograft augmented with VFG and followed up minimum 1 year were evaluated for bone union, functional result and complications. The influence of various factors on bone union and functional outcomes were also analyzed.

Results: Bone unions were obtained at 13 of 20 junctions. Average union time was 3.7 months at metaphyseal junctions and 8 months at diaphyseal junctions (P<0.05). At diaphyseal junctions, younger aged group and intramedullary location group showed earlier bone union (P<0.05). The mean functional score was 81%. There were 3 nonunions, 4 delayed unions and 2 recycled bone resorption combined with fractures.

Conclusion: To obtain excellent results, proper microvascular technique, sufficient length of VFG bridging both junctions, stable internal fixation and protection of reconstructed bone until union are necessary.
KEYWORD
Bone defect, Recycled autograft, VFG, Bone union, Functional outcome, Complication