Lousiness Improving on the Refining Process
Kim Byong-Ho

Chung Jin-Yong
Abstract
This experiment is to investigate the influence on business by varying the scouring condition of raw silk. The conditions of experiment are changed by temperature, time concentration and scouring reagent as well as the pH value of scouring solution, involving the repeat number of treatment in the same reagent solution. The results are as follows. 1) The shorter the scouring time, the more lousiness showed on law silk. The difference of lousiness quantity are especially remarkable between 30 min. and 60min, while the appearance of lousiness is slight between 50min. and 90min. 2) The lousiness shape was just like splited end and short wool fiber type during than 60 min. scouring, and splited end and long wool fiber type was appeared during 120 min. scouring. 3) The seperation of threads on silk panel was difficult with undissolved sericin in case of lower than 90 of scouring temperature, so that it was almost impossible to inspect lousiness. 4) In case of repeating one after another scouring in the same solution, the more number of treatment, the less sho wed lousiness. Little difference were appeared in the quantity of lousiness from first to eighth repeated scouring, while large difference of quantity was appeared between 8th and 9th repeated scouring. 5) The quantity of lousiness was also increased until scouring reagent (Marseilles soap) is added to 0.75£¥, but rather decreased with more than 0.75£¥ of soap. The most variety of lousiness quantity was occured when the concentration of soap is changed from 0.15£¥ to 0.20£¥. 6) The peculiarities of lousiness shape by the concentration of scouring reagent were as followings; most of lousiness are splited end short wool fiber type with lower wool fiber type with higher than 0.75£¥, and the mixture of both the former and the latter with 0.5£¥ concentration. 7) The quantity of lousiness by the kind of scouring reagent was the least with 5£¥ of NaCO solution, and the most with the mixture of 0.25£¥ Marseilles soap and 0.25£¥ NaCO. 8) The more increased pH value, the more lousiness showed. The peculiarities of lousiness shape was the splited end and short wool fiber type, and the end and long wool fiber type with higher value of pH 11 because of the decreased strength of threads and the cutting of brin. 9) With the discussions mentioned the above, the scouring conditions to decrease the lousiness quantity are summarized as follows. (1) It is better to take the possible long time of scouring. (2) Temperature should be kept higher than 95 for complete scouring. (3) It was the best to use 0.5£¥ of Marseiles soap as scouring reagent. (4) No good results were produced by using the mixture of scouring reagent. (5) The best pH range of scouring solution was 9.5 to 10.5.
KEYWORD
FullTexts / Linksout information
Listed journal information