Unfolded Histidine-Tagged Protein is Immobilized to Nitrilotriacetic Acid-Nickel Beads, But Not the Nickel-Coated Glass Slide
Cho Min-Ho

Ahn Sun-Young
Park Heon-Yong
Abstract
The adsorption of proteins on the surface of glass slides is essential for construction of protein chips. Previously, we prepared a nickel-coated plate by the spin-coating method for immobilization of His-tagged proteins. In order to know whether the structural factor is responsible for the immobilization of His-tagged proteins to the nickel-coated glass slide, we executed a series of experiments. First we purified a His-tagged protein after expressing the vector in E. coli BL21 (DE3). Then we obtained the unfolding curve for the His-tagged protein by using guanidine hydrochloride. Fractions unfolded were monitored by internal fluorescence spectroscopy. The ${\Delta}G_{H20}$ for unfolding was $2.27kcal/mol{/pm}0.52$. Then we tested if unfolded His-tagged proteins can be adsorbed to the nickel-coated plate, comparing with $Ni^{2+}-NTA$ (nitrilotriacetic acid) beads. Whereas unfolded His-tagged proteins were adsorbed to $Ni^{2+}-NTA$ beads, they did not bind to the nickel-coated plate. In conclusion, a structural factor is likely to be an important factor for constructing the protein chips, when His-tagged proteins will immobilize to the nickel-coated slides
KEYWORD
his-tagged protein, nickel-coated glass slides, protein chip, unfolding
FullTexts / Linksout information
Listed journal information
ÇмúÁøÈïÀç´Ü(KCI) KoreaMed