Restorative management using hybrid ceramic of a patient with severe tooth erosion from swimming: a clinical report
Chaimongkon Peampring

Abstract
This clinical report presents the clinical appearance and treatment approach in a case of excessive anterior teeth erosion resulted from swimming in a poorly-chlorinated swimming pool. Clinical findings revealed tooth sensitivity, severe enamel erosion resembling veneer preparations, and the presence of anterior open bite. A novel hybrid ceramic (Vita Enamic) was chosen for fabricating full-coverage crowns for this patient. After 6-months follow-up, the tooth sensitivity disappeared and the patient was satisfied with esthetic outcome. The hybrid ceramic restorations can be recommended with no complications.
KEYWORD
Dental erosion, Swimming, Hybrid ceramic, Vita enamic
FullTexts / Linksout information
 
Listed journal information
SCI(E) ÇмúÁøÈïÀç´Ü(KCI) KoreaMed