Metal stain on monolithic zirconia restoration: A case report
Cha Min-Sang

Lee Sang-Woon
Huh Yoon-Hyuk
Cho Lee-Ra
Park Chan-Jin
Abstract
In restorative treatment using fixed dental prostheses, dentists should select appropriate restoration material among various types of dental materials. The strength, marginal fit, esthetics, wear resistance, biocompatibility, and cost are important factors in the choice of restoration materials. The present case showed a surface stain on a monolithic zirconia restoration that was due to wear between the monolithic zirconia restoration and the base metal alloy restoration. This phenomenon was confirmed by surface roughness measurement and electron probe micro-analysis.
KEYWORD
Zirconia, Stain, Dental alloy, Wear